Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Kraton D1184 AIM - SBS - Kraton Polymers

Material Data Center offers the following functions for Kraton D1184 AIM:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Kraton D datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
Kraton D1184 A is a clear, branched block copolymer based on styrene and butadiene with bound styrene of 30% mass.
Kraton D1184 AIM - supplied as powder dusted with calcium carbonate.
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ISO Data
Indice de fluidité, MFI 1 g/10min ISO 1133
Température 200 °C -
Charge 5 kg -
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Résistance à la traction 27 MPa ISO 37
Déformation à la rupture 820 % ISO 37
Dureté Shore A 75 - ISO 7619-1
Other Standards[S]
Contrainte à 300% de déformation 7.5 MPa ISO 37
S: These properties are reported by the producer according standards that are different to our defaults.
Propriétés diversesValeurUnitéNorme du test
Bulk density 400 kg/m³ -
Other Standards[S]
Masse volumique 940 kg/m³ ISO 2781
S: These properties are reported by the producer according standards that are different to our defaults.
Caractéristiques
Transformation
Enduction
Conditionnement
Poudre
Propriétés spéciales
Transparent
Caractéristiques
Copolymère
Résistance Chimique
Résistance à oxydation
Disponibilité régionale
Amérique du nord
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.